Technical data sheet ASODUR®-G1270 Versatile epoxy resin
Material number
Contents
Unit of quantity
Packaging
Colour
206404004
30
KG
Set
Transparent
206404003
10
Combination packs
206404002
3
206404005
532
Product features Two component resistant to diluted alkaline solutions, acids, aqueous salt solutions, lubricants Solvent free withstands mechanical loading Low viscosity pore filled water resistant
Advantages Transparent consolidating
Areas of application / surface protection as impregnation for substrate consolidator for pore blocked priming of cement-based surfaces for the production of levelling and scratch coat material for the production of epoxy resin screeds and mortars
SCHOMBURG GmbH & Co. KG · Aquafinstr. 2–8 · D-32760 Detmold (Germany) · Tel. +49-5231-953-00 · Fax +49-5231- 953-333 · schomburg.com 1/6
10/03/2025
Technical data sheet ASODUR®-G1270 Existing test certificates Reaction to fire DIN 13578
Technical Data Material properties Product components Base material Consistency Density, ready to use product (ISO 1183-1) Flexural strength of the (screed) mortar Compressive strength (DIN EN 196-1) Tensile adhesion strength (concrete, dry until matt damp) Viscosity, ready to use product [value] Classification of the reaction to fire in accordance with DIN EN 13501-1
2 component system Epoxy resin Liquid approx. 1.08 g/cm³ approx. 40 N/mm² approx. 50 N/mm² ≥ 1.5 N/mm² approx. 130 mPa*s Efl
Mixing Mix ratio, component A Mix ratio, component B Mix ratio, addition of ASO-FF levelling / scratch coat Mix ratio, addition of levelling / scratch coat quartz sand Mix ratio epoxy resin mortar 11-150 mm (quartz sand Ø 0.06-3.5 mm) Mix ratio epoxy resin mortar 5-30 mm (quartz sand Ø 0.06-1.5 mm) Mixing time
100 weight proportion 27 weight proportion approx. 0.02 - 0.03 weight proportion 1 weight proportion approx. 8.3 weight proportion approx. 8.3 weight proportion approx. 3 minutes
Application approx. 10 - 35 °C Substrate temperature 80 % Max. relative humidity approx. 30 minutes Pot life min. 10 °C Minimum reaction temperature Drill with stirrer Mixing method, machines, tools approx. 0.30 - 0.60 kg/m² Consumption approx. 12 hours Second application step after waiting time after 12 hours Overcoat after (min.) Consumption per mm layer thickness (levelling and scratch coat with quartz sand) approx. 1.6 kg/m² approx. 12 hours Foot traffic after approx. 2 kg/m² Consumption (epoxy resin screed 5-30 mm per mm layer thickness) approx. 2 kg/m² Consumption (epoxy resin screed 11-150 mm per mm layer thickness) approx. 10 - 35 °C Application temperature to 24 hours Overcoat after (max.) approx. 7 days Hardening time / full resilience
Processing equipment Aids/tools Rubber lip slider Stirrer (approx. 300 rpm) Circular cage Nylon fur roller (6mm) with textured polyamide cover
SCHOMBURG GmbH & Co. KG · Aquafinstr. 2–8 · D-32760 Detmold (Germany) · Tel. +49-5231-953-00 · Fax +49-5231- 953-333 · schomburg.com 2/6
Technical data sheet ASODUR®-G1270 Manual processing distributable with rubber lip slider Distributable with nylon fur roller
Preparing the substrate Requirement for substrate 1. Dry 2. Load-bearing 3. Firm 4. Grippy 5. Free of adhesion inhibiting substances 6. Protected from moisture penetration from the rear
Measures for substrate preparation Substrate preparations must be carried out in compliance with DIN EN 14879-1:2005, 4.2 et.seq.
Substrate quality class
Application Mixing 1. The (ideal) material temperature during the mixing procedure is +15 °C. 2. Add the hardener to the resin. 3. The hardener must run completely out of the container. 4. Mix thoroughly with the mixer until a homogeneous consistency. 5. The hardener must be distributed evenly. 6. The mixing time is ca. 3 minutes. 7. Decant the mass into a clean bucket. 8. Stir carefully again. 9. When adding quartz sands, make sure that they are kiln-dried and, like other aggregates, also have a temperature of approx. +15 °C.
Production and application of levelling compound/scratch coat material: 1. Prime the substrate with ASODUR®-G1270. 2. The quartz sand (Ø 0.1-0.6 mm) is mixed into the previously homogeneously mixed and re-potted resin and hardener component (mix ratio 1:1). 3. Mix the liquid and solid components evenly. 4. For levelling/scratch coats on vertical and sloping surfaces, we recommend the addition of 2-3% wt. ASO®-FF. 5. Apply the mixed levelling/scratch coat in a single application step using the scratch filler method. 6. Sprinkle the still fresh levelling/scratch coat with quartz sand (Ø 0.1 - 0.6 mm). 7. Consumption of mixture for scratch coat approx. 1.6 kg/m² per mm layer thickness
Application 1. ASODUR®-G1270 is applied generously to the prepared substrate with a suitable tool. 2. The filler mortar is to be prepared with the priming resin with the addition of quartz sand. 3. The fresh primer is sprinkled with quartz sand (Ø 0.1-0.6 mm) to cover the entire surface. 4. The second layer can be applied with a dense smoothing mortar. 5. After the sanded layer has cured, the unbound quartz sand is meticulously removed before the next application step. 6. After a waiting time of approx. 12 to 24 hours, work can continue with an ASODUR® coating system or the floor covering structure. 7. Irregularities lead to capillary-active pores and facilitate the formation of bubbles. 8. To ensure a pore blocked primer coat, apply the primer in two layers.
SCHOMBURG GmbH & Co. KG · Aquafinstr. 2–8 · D-32760 Detmold (Germany) · Tel. +49-5231-953-00 · Fax +49-5231- 953-333 · schomburg.com 3/6
Technical data sheet ASODUR®-G1270 Primer 1. apply flowing and pore sealed ASODUR®-G1270. 2. Apply the material in 1-2 application steps. 3. The second application step is to be performed after a waiting time of at least 12 hours within a further 24 hours. 4. Re-coat the primed, non-sanded surface within 12-24 hours. 5. Sprinkle the two layers of primer with quartz sand. 6. After the sanded layer has cured, the unbound quartz sand is meticulously removed before the next application step. 7. Only walk on non-sanded primer with clean overshoes. 8. If quartz sand is used, the primer must be applied in two application steps.
Mixing and applying of the epoxy resin coating 1. Add the quartz sand (Ø 0.06 - 1.5 mm) in the correct quantity (3:25) to the forced paddle mixer (e.g. type: Zyklos or UEZ). 2. Then add the mixed resin mixture. 3. Mix the liquid and solid components evenly. 4. Prime ASODUR®-G1270 using the roller method. 5. Consumption approx. 0.3 kg/m² 6. The mixed screed is applied to the still fresh primer in a layer thickness of at least approx. 5 mm, drawn off with gauges and mechanically smoothened. 7. Consumption of screed mix approx. 2 kg/m² per mm layer thickness
Producing and application of the epoxy resin screed (layer thickness from 11 to 150 mm) 1. Add the quartz sand (Ø 0.06 - 3.5 mm) in the correct quantity (3:25) to the forced paddle mixer (e.g. type: Zyklos or UEZ). 2. Then add the mixed resin mixture. 3. Mix the liquid and solid components evenly. 4. Prime ASODUR®-G1270 using the roller method. 5. Consumption approx. 0.3 kg/m² 6. The mixed screed is applied to the still fresh primer in a layer thickness of at least approx. 5 mm, drawn off with gauges and mechanically smoothened. 7. Consumption of screed mix approx. 2 kg/m² per mm layer thickness
Producing and applying epoxy mortar as a levelling and coving mortar 1. Stir the quartz sand (Ø 0.06-1.5 mm) homogeneously into the mixed ASODUR®-G1270 in a mix ratio of 3:25. 2. Prime the substrate with ASODUR®-G1270. 3. Apply the mortar while still wet using trowel techniques, ensuring even compaction.
Cleaning tools Clean tools immediately after use with suitable solvent.
Storage conditions Storage Store in a frost-free, cool and dry place. At min. 10 - 25 °C for 24 months in the original canister. Promptly use opened container.
Disposal Hardened product leftovers can be disposed of in accordance with disposal code AVV 15 01 06.
SCHOMBURG GmbH & Co. KG · Aquafinstr. 2–8 · D-32760 Detmold (Germany) · Tel. +49-5231-953-00 · Fax +49-5231- 953-333 · schomburg.com 4/6
Technical data sheet ASODUR®-G1270 Notes The indicated consumption quantities are calculated values without additions for textured surface roughness and absorbency, level compensation and residual material in the container. We always recommend a calculated safety addition of 10% on top of the calculated consumption quantities. Higher temperatures shorten the pot life. Lower temperatures increase the application and hardening times. The rate at which material is consumed also increases at lower temperatures. The bonding between the individual layers can be strongly disrupted between the individual application steps due to the effects of dampness and contamination. Coating work requires a substrate temperature of at least 3 °C above the dew point temperature. If longer waiting times arise between the individual application steps or surfaces that have already been treated with liquid resin are coated again after an extended period of time, the old surface must be well cleaned and thoroughly roughened. Then apply a complete pore-free new coating. Ensure there is good ventilation during the drying and hardening phases. After they have been applied, surface protection systems must be protected against dampness (e.g. rainwater, condensation water) for approx. 4–6 hours. Moisture causes a white colour and/or stickiness on the surface and can cause problems during hardening. Discoloured and/or sticky surfaces must be removed and reworked, e.g. through grinding or shot blasting. If organic acids (e.g. propionic acid) are used or present in mobile silo systems, ASODUR®-G1270 must not be used as the sole waterproofing and surface protection measure. ASODUR®-G1270 must be coated with a top coat adapted to the usage requirements. For vertical surfaces use ASODUR®-G1270 with the addition of ASO®-FF. Observe the technical data sheets of the products mentioned before starting work. Applications that have not been clearly mentioned in this technical data sheet may only be carried out after the technical service department of SCHOMBURG GmbH has been consulted, and after the said department has approved of such a course of action in writing. For detailed information on application, read and observe supplementary technical information no. 19 "Applying ASODUR® products".
Relevant regulations The recognised standards of construction engineering, the relevant guidelines and current regulations must be observed. Observe applicable safety data sheet! GISCODE: RE 90 Explanations Conformity / Declaration / Verification
SCHOMBURG GmbH & Co. KG · Aquafinstr. 2–8 · D-32760 Detmold (Germany) · Tel. +49-5231-953-00 · Fax +49-5231- 953-333 · schomburg.com 5/6
Technical data sheet ASODUR®-G1270 Chemical durability
The rights of the buyer with regard to the quality of our materials are based on our terms and conditions of sale and delivery. Our technical advice team will be happy to advise you in the case of requirements that exceed the scope of the application described here. In order to be binding, a legally binding written confirmation is required. The product description does not release the user from a duty of care. Lay a test area in the event of uncertainty. This version becomes invalid in the event of a new version being issued.
SCHOMBURG GmbH & Co. KG · Aquafinstr. 2–8 · D-32760 Detmold (Germany) · Tel. +49-5231-953-00 · Fax +49-5231- 953-333 · schomburg.com 6/6